Large sign splits and slicer bed setup
When one letter is larger than the bed, the split decides the quality. Lock the split line, the joint tolerance, and the placement in the model, then send it to the slicer. A slicer cut does not replace locating pins.
Starting speeds are in High-speed profiles. Extra finishing time from the split goes into Pricing.
Usable bed by machine
Quote and split against the usable side length, after brim, skirt, and purge line.
| Machine | Official bed (mm) | Recommended usable side | Notes |
|---|---|---|---|
| Bambu Lab X1 / P1 series | 256 × 256 × 256 | 236–240 | Textured PEI, after flow calibration |
| Bambu Lab A1 | 256 × 256 × 256 | 236–240 | Open frame. Watch large flat parts in a draft |
| Creality K1 / K1C | 220 × 220 × 250 | 200–205 | After input shaper is done |
| Creality K1 Max | 300 × 300 × 300 | 280–285 | Check corner level and shrinkage |
Treat the height limit as official Z minus 10 mm for the cable chain and clips.
Split rules
- Put the split line where the stroke is thick, not at the thinnest neck.
- Do not cross the middle of a visible face. Hide the joint on a side, a rear flange, or a stroke intersection.
- Keep the longest side of one part at or below
usable side − brim (5–8 mm per side × 2). - Do not rely on a straight butt joint alone. Add at least two locating features.
- Engrave the part number, a direction arrow, and an up mark on the back. Height 0.4 mm, stroke width at least 0.6 mm.
| Letter condition | Split | Why |
|---|---|---|
| One side is within the usable length | Do not split | Joint tolerance costs more than it saves |
| Only one direction exceeds the bed | One cut | Two pins plus a rear flange |
| Both directions exceed the bed | A grid split | Keep a crossing joint off a single line |
| Serifs or tips are weak | Keep the tip in one piece | A split at the tip breaks, and it shows as a step |
Joints and tolerance
Baseline: 0.4 mm nozzle, with outer-wall speed at or below the outer-wall cap in the high-speed profile. Values are labeled as diameter or per-side clearance, not left ambiguous. Confirm one coupon set before production.
| Joint | Starting design | A good fit | How it fails |
|---|---|---|---|
| Dowel pin Ø4.0 | Hole Ø4.25–4.40 | Goes in by hand and does not rattle | An undersize hole spreads the part |
| Dowel pin Ø6.0 | Hole Ø6.30–6.50 | Same | Default pin for a large channel |
| Dovetail | 0.15 mm clearance per side | Play of 0.3 mm or less after it slides | Zero clearance stops on layer lines |
| Tongue and groove | 0.15–0.20 mm clearance per side | Use with a rear screw or adhesive | A tongue under 2 mm thick breaks |
| Rear overlap flange | Overlap 12–20 mm, screw pitch 40–60 mm | From the front, only the joint line shows | Overlap under 8 mm leaves a step |
| Butt joint plus adhesive | Mating-face gap 0.10–0.20 mm | The adhesive layer does not push the faces apart | A zero-gap design bulges |
Model pin holes as vertical walls, and align the axis with Z so slicer support does not grow inside the hole. For a horizontal hole, use a teardrop (a flattened top) or orient the pin axis with the print direction.
For PETG and ASA, start 0.1 mm larger than the PLA coupon hole and measure again.
Slicer bed setup
| Item | Setting | Why |
|---|---|---|
| Origin | Bed center | Avoids corner temperature difference |
| Spacing | At least 6 mm between parts. Brims must not overlap | Stops fused brims and nozzle crashes |
| Large visible face | On the bed when you can | The first layer is the most even face |
| Seam | Rear, or an aligned seam | A random seam on the front becomes a vertical line |
| Support | Keep it out of joint grooves | Leftover support destroys tolerance |
| Brim | Only on tall, narrow strokes, 5–8 mm wide | A brim on every part adds finishing time |
| Order | Do not park a fragile outline inside the group | A fallen part scrapes its neighbor |
| Purge / prime | Separate from the model outline | On a K1, check that the prime line does not stick to the brim |
After placement, scrub only the locating-pin layers in the slicer preview. If a bridge is floating inside the hole, do not print that part. Rotate the axis.
Numbering and the assembly map
- File name:
sign_part_rowcol_material_nozzle, for exampleACME_A_R1C2_PETG_04 - Rear engraving: the short form of the same code,
A12 - One assembly sheet is enough: the split lines drawn on a front photo. Keep it on the job ticket, separate from the customer installation sheet.
- Dry-fit and measure the full width before adhesive. If the width is off the drawing by more than ±1.0 mm per meter, decide whether the error is stacked joint gaps or shrinkage, then correct the remaining parts.
Record the hole diameter that passed the coupon, with the machine name, in the job log. The next order starts its split tolerance from that value.